- Size: 0.01
- Place of Origin: China
- Brand Name: FULLWORLD
- Model Number: FWH90
- Weight: 0.090 kg
| Welding flux sizes | Weight |
| FWH090 | 90g |
| FWH115 | 115g |
| FWH150 | 150g |
| FWH200 | 200g |
| FWH250 | 250g |
Of course , we can package it according to your requirement .
- Size: 0.01
- Place of Origin: China
- Brand Name: FULLWORLD
- Model Number: FWH90
- Weight: 0.090 kg
Exothermic welding materials welding flux
1,Current carrying capability from welding point is same as conductor with good conducting performance. After inspection, the DC resistance ratio and change rate
are almost zero before and after welding. This is the level that any of the traditional
welding method cannot be compared
2, No need of resources from outside. It can be operated indoor and outdoor
3, It won't be damaged by surge current. The test shows the conductor will be melted
earlier than welding points when under high current impact in short period
4, Corrosion or slack will not be produced from welding. As it is weld junction,no
contact surface, no residual stress, junction is stable and reliable as long term
conductive body
5, As it is welding junction, connector and conductor are combined on molecular.So
it has a good mechanical strength and is a permanent junction
6, Equipment is simple, convenient and handy. The operation is easy and can be done
without professionals
Company Information
Established in 2005 with 10,000,000 RMB registered capital .We already have more than ten tears experience .
We could provide you the Copper bonded Steel Earth Rod ,Copper Bonded Steel Tape ,chemical ground electrode ,exothermic welding material ,and other earthing accessories and material .With our own factory and professional team , we could provide you the best products and service .
Why choose us ?
1:10 years of R&D
2:Experience engineers and project teams .
3:Quality Approvals
4:Reasonable Price
5:Fast Delivery
6:Perfect after-sales Service
7:Small Orders Accepted
Any query or questions ,please feel free to contact me .